SA 213 T22

 ferritic and austenitic  boiler, superheater, and heat exchanger .
Chemical Properties:
Carbon: 0.05min-0.15max.Silicon: 0.50 max.
Manganese: 0.30-0.60Nickel: n/a
Potassium: 0.025Chromium: 1.90-2.60
Sulfur: 0.025Molybdenum: 0.87-1.13
Mechanical Properties:
Tensile Strength:
ksi: 60
MPa: 414
Yield:
ksi: 30
MPa: 207
Elongation in 2in. or 50mm, min. %: 30
Max. Hardness Rockwell B: 85