SA-209-T1B

 have a typical chemistry with additions of 0.44-0.65 Molybdenum. Bearing minimum tensile strength of 415 Mpa ASME SA 209 Grade T1b Tubes have a minimum yield strength of 220 Mpa.
Seamless carbon molybdenum  boiler and superheater tubes.
Chemical Properties:
Carbon: 0.14 maxSilicon: 0.10-0.50
Manganese: 0.30-0.80Nickel: n/a
Potassium: 0.025Chromium: n/a
Sulfur: 0.025Molybdenum: 0.44-0.65
Mechanical Properties:
Tensile Strength:
ksi: 53
MPa: 365
Yield:
ksi: 28
MPa: 193
Elongation in 2in. or 50mm, min. %: 30
Max. Hardness Rockwell B: 77